Adhering to scientific and technological innovation for development, the company has established a research and development team led by many doctors, and built a 1000 square meters research and development laboratory; We have established a complete quality control system and management team, and applied for ISO9001 quality system certification and ISO14001 environmental management system certification.
1.Product Introduction
Photovoltaic EVA packaging film is made of ethylene-vinyl acetate copolymer (EVA) with various necessary additives. Its main functions in the packaging of solar cells are: supporting and fixing solar cells; Increase the transmittance of sunlight; Resist the damage of the external environment on the performance of the battery and protect the battery; The product has the following characteristics:
A. Excellent peel strength after aging to ensure that outdoor components do not delaminate for 25 years;
B. Excellent stability and product compatibility;
C. Good operability, easier lamination, short lamination time and high efficiency;
D. Superior weather resistance (including high temperature, high humidity, ultraviolet, etc.), PID resistance;
E. Excellent light transmittance ensures the maximum power of the module.
The main models are:
A. BJ-920 (high transmittance PID): BJ-920 has high transmittance in the ultraviolet light area, and the light transmittance in the ultraviolet area is ≥ 80%. When used, it is close to the glass surface. Compared with ordinary EVA film, it can more effectively improve the conversion efficiency of the module by 1.5% - 5%; B. BJ-921 (high cut-off resistance PID): the light transmittance in the ultraviolet area is ≤ 30%, and the back panel surface can effectively prevent the back panel from being damaged by ultraviolet light, slow down the aging speed and extend the service life of the module.
2.Product technical parameters:
Performance | Model | ||
BJ-920 | BJ-921 | ||
Thickness(mm) | 0.3-1.0 | 0.3-1.0 | |
Width(mm) | ≤1400 | ≤1400 | |
Roll length(m) | 150-350 | 150-350 | |
Area density deviation(%) | ±4 | ±4 | |
Density(g/cm3) | 0.95-0.96 | 0.95-0.96 | |
Crosslinking degree(%) | ≥75 | ≥75 | |
Tensile strength(MPa) | ≥18 | ≥18 | |
Elongation(%) | ≥500 | ≥500 | |
Water absorption(20℃,、24h) | ≤0.1% | ≤0.1% | |
Peel strength from glass(N/cm) | ≥60 | ≥60 | |
Peel strength from backplane(N/cm) | ≥40 | ≥40 | |
Shrinkage(%) | Direction(MD) | ≤3.0 | ≤3.0 |
Droadwise(TD) | ≤1.5 | ≤1.5 | |
Volume resistivity(Ω·cm) | ≥1*1015 | ≥1*1015 | |
Breakdown voltage strength (kv/mm) | ≥26 | ≥26 | |
UV aging △YI (120kwh/m2,1000 h) | ≤4 | ≤4 | |
Damp-heat aging △YI (85℃/85%,,1000 h) | ≤4 | ≤4 | |
Transmittance(%) | 380-1100nm | ≥91 | ≥91 |
290-380nm | ≥80 | ≤30 |
3.Lamination process:
3.1Single-cavity lamination parameters
Product model | Lamination temperature(℃) | Vacuum pumping time(s) | Holding pressure | Holding time | ||
one paragraph | Section II | three-section | ||||
BJ-920 | 142±2 | 360±60 | -70 | -45 | -20 | 600-660 |
BJ-921 | 142±2 | 360±60 | -70 | -45 | -20 | 600-660 |
3.2<spanDouble cavity lamination parameters
Product model | First chamber temperature(℃) | Vacuum pumping time(s) | Holding pressure | Holding time | Second chamber temperature(℃) | Vacuum pumping time(s) | Holding pressure | Holding time | ||||
one paragraph | Section II | three-section | one paragraph | Section II | three-section | |||||||
BJ-920 | 122±2 | 360±60 | -70 | -45 | -20 | 180±30 | 145±2 | 30±10 | -70 | -45 | -20 | 480±60 |
BJ-921 | 122±2 | 360±60 | -70 | -45 | -20 | 180±30 | 145±2 | 30±10 | -70 | -45 | -20 | 480±60 |
Note: According to the operation of the customer's equipment, the temperature and time of the laminator can be adjusted appropriately to meet the production requirements. The crosslinking degree shall be controlled within the acceptable range, and 85% is the best. Other auxiliary materials used shall be qualified products tested by the industry recognized testing agency.
4,、 Storage and use:
1. Store in a cool and dry constant temperature room with temperature ≤ 30 ℃ and humidity ≤ 60%; The storage period of this product is six months; It is recommended to use it within three months;
2. Vacuum packaging, inner packaging 150-300m/roll (except for special requirements);
3. The long-term stacking height of products is not easy to be too high, and it is better to store products below five layers to avoid bending and deformation caused by heavy pressure;
4. Do not damp the product. It is recommended to use the plastic film after opening the package or cutting it within 48 hours;
5. In order to avoid abnormal lamination of components caused by static electricity, it is recommended to eliminate static electricity in the whole process of component production.